Question:

Boron and silicon of very high purity can be obtained through :

Show Hint

Semiconductor-grade B and Si (ultra pure) are refined by melting a narrow zone of the rod and sweeping it along so that impurities collect in the molten zone.
Updated On: Nov 5, 2026
  • Liquation
  • Electrolytic refining
  • Zone refining
  • Vapour phase refining
Show Solution
collegedunia
Verified By Collegedunia

The Correct Option is C

Solution and Explanation

Liquation is used for low-melting metals such as Sn and Pb. Electrolytic refining is used for metals like Cu, Ag, Al. Vapour phase refining (Mond and van Arkel methods) is used for Ni, Zr, Ti.
Elements needed in extremely high purity as semiconductors (Si, Ge, B, Ga, In) are purified by zone refining. A circular heater moves along a rod of the impure element; impurities are more soluble in the melt than in the solid, so they are swept to one end of the rod.
Answer: (3) Zone refining
Was this answer helpful?
0
0