Question:

Blow holes are casting defects caused by

Show Hint

Proper venting of molds and careful control of the molten metal's temperature can help minimize the occurrence of blow holes during casting.
Updated On: May 6, 2025
  • Excessive gaseous substances not able to escape
  • Discontinuity in metal casting resulting from hindered contraction
  • Two streams of metals that are too cold to figure properly
  • Some sand shearing from the cope surface
Show Solution
collegedunia
Verified By Collegedunia

The Correct Option is A

Solution and Explanation

Blow holes in casting are caused by the entrapment of gases, which cannot escape from the molten metal during solidification, leading to defects in the final casting.
Was this answer helpful?
0
0